EP55TCFL Product Description

One component, pre-mixed and frozen epoxy featuring high thermal conductivity and good electrical insulation

UV18Med-2 Product Information

One Component, UV Curable System with Outstanding Chemical Resistance for High Performance Bonding and Coating. Meets ISO 10993-5 Specifications for Medical Applications.

UV10TK40RCL Product Information

High Viscosity, One Component, UV Curable Epoxy Acrylate for High Performance Bonding, Coating and Sealing that turns from red to clear upon exposure to UV light. with Exceptional Thermal Stability and Very Low Shrinkage upon Cure.

EP3HTND-2 Black Product Information

One Component, Epoxy System for Bonding, Sealing and Coating Featuring Very Fast Cure along with High Shear Strength Properties. Meets USP Class VI Specifications.

UV23FLDC-80 Product Information

One component, low viscosity, dual curing, cationic type system. Good flexibility. Serviceable from -80°F to 300°F.

Supreme 17HTMed Product Information

One component, medical grade toughened epoxy system for bonding and sealing

MasterSil 153AOMed Product Information

MasterSil 153AOMed Two Part Medical Grade Silicone

Two part medical grade silicone for high performance bonding and sealing