112 products match
![]() |
EP19HTLV-2 Viscosity 200-700 cps. One part system has "unlimited" working life at room temperature. Impressive physical strength properties. Sprayable or brushable. Chemical resistant. Excellent thermal stability. Serviceable from -60°F to +400°F. |
![]() |
EP3 One component heat curable epoxy adhesive. Fast cure speeds. Resists vibration, impact, stress fatigue cracking, creep corrosion. Gray color. Adhesive spreads evenly and smoothly. Serviceable from -100°F to +300°F. |
![]() |
EP36 One part B-staged epoxy. Flexibilized and toughened. Withstands rigorous thermal cycling and thermal shocks. Superb electrical insulation properties. Ideal for potting/encapsulation. Serviceable from -100°F to +500°F. Available in 30 gram cookies. |
![]() |
EP36AN Thermally conductive/electrically insulative B-stage epoxy potting/bonding compound. Outstanding toughness and flexibility. Resists up to 500°F. Ability to withstand thermal cycling and impact/vibration. Shore D hardness 80. Volume resistivity 1014 ohm-cm. |
![]() |
EP36AO Thermally conductive, electrically insulative B-stage toughened epoxy. One part system. Ideal for potting and encapsulation. Capable of withstanding rigorous thermal shocks. Serviceable from -100°F to +500°F. Available in 30 gram cookies. Meets NASA low outgassing specifications. |
![]() |
EP36CLV One component, B-staged epoxy. Features low viscosity and excellent electrical insulation properties. Operating service temperature range -100°F to +500°F. Combines flexibility and toughness. Superior chemical resistance to water, acids, bases, fuels and oils. Elongatio >50%. |
![]() |
EP36FR Flame retardant B-stage toughened epoxy. One part system. Ideal for potting and encapsulation. Capable of withstanding rigorous thermal shocks. Serviceable from -100°F to +500°F. Available in 30 gram cookies. |
![]() |
EP3ANHT Heat resistant thermal conductive epoxy for potting and bonding. No mix system. 100% reactive. Thermal conductivity 23 BTU in/ft2/hr/°F. Gel time 90-100 seconds at 150°C. Volume resistivit <1015 ohm-cm. Offers protection against abrasion and thermal cycling. Serviceable from -60°F to +400°F. |
![]() |
EP3AOHT Light paste. One component, no mix system. Thermally conductive/electrically insulative. Service temperature range -60°F to +400°F. Flexible cure schedules. Cost effective. |
![]() |
EP3AOHTLV Single component thermally conductive/electrically insulative epoxy for bonding/potting. Heat resistant. Fast curing. Offers excellent adhesion to metallic and nonmetallic substrates. Serviceable from -60°F to +400°F. |